Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 147.63 g/mol
147.63 g/mol
Descriptive Properties Value Comments
Assay 59% Sr
CAS Number 1633-05-2
Form White powder
Purity 99.999%
Typical Impurities Ba, Ca < 6; Mg < 1 ppm