DuPont Performance Polymers AquaStik® 2901 Latex  (discontinued **)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers AquaStik® 2901 Latex  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: AquaStik® 2901 contains a high modulus, fast crystallizing polychloroprene homopolymer made in an anionic colloidal system.Main Feature: This latex is resistant to low temperature exposure, and gives adhesives with very fast strength development.Suggested End Uses:Adhesives for bonding foam to various substratesFoam adhesivesFabric saturantsInformation provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Latex at 25°C
Density 1.23 g/cc
0.0444 lb/in³
Polymer
Particle Size 0.13 µm
0.13 µm
Average
pH 12.5
12.5
25°C
Brookfield Viscosity >= 6.00e+7 cP

@Temperature 25.0 °C
>= 6.00e+7 cP

@Temperature 77.0 °F
6 rpm or 30 rpm
Surface Tension 37.6 dynes/cm
37.6 dynes/cm
Descriptive Properties Value Comments
Electrolyte Stability Fairly Good
Emulsifying Agent Potassium salt of resin acid
Freeze/thaw Resistant to -5°C
Mechanical Stability Good
Polymer Type Fast Crystallizing Homopolymer
Solids 56-60 wt%
Storage Good