Polymer Property : Brookfield Viscosity = 6.00e+7 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity >= 6.00e+7 cP

@Temperature 25.0 °C
>= 6.00e+7 cP

@Temperature 77.0 °F
6 rpm or 30 rpm
DuPont Performance Polymers AquaStik® 2901 Latex  (discontinued **)
Description: AquaStik® 2901 contains a high modulus, fast crystallizing polychloroprene homopolymer made in an anionic colloidal system.Main Feature: This latex is resistant to low temperature expo..