Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvaloy® 742 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvaloy® 742 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792 - ISO 1183
Melt Flow 25 - 45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25 - 45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
ASTM D2240 - ISO 868
Tensile Strength at Break 4.20 MPa
609 psi
ASTM D638 - ISO 527-2
Elongation at Break 1200 %
1200 %
ASTM D638 - ISO 527-2
Thermal Properties Metric English Comments
Melting Point 45.0 °C
113 °F
ASTM D3418 - ISO 3146
Glass Transition Temp, Tg -32.0 °C
-25.6 °F
ASTM D3418