Dow VORANOL™ CP 1421 Polyol

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name VORANOL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow VORANOL™ CP 1421 Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VORANOL™ CP 1421 polyol is a polyether polyol especially designed for the production of soft and hypersoft flexible slabstock foams. It is also used at low level (0.5 to around 5 php) as cell opener in high resilience slabstock and molded foam.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.091 g/cc
1.091 g/cc
pH 5.5 - 8.0
5.5 - 8.0
(1 Water / 10 Methanol); DOWM 101495-TE94A
Viscosity Measure 655 cSt

@Temperature 37.8 °C
655 cSt

@Temperature 100 °F
ASTM D445-94
1190 - 1420 cSt

@Temperature 25.0 °C
1190 - 1420 cSt

@Temperature 77.0 °F
ASTM D445-94
Maximum Moisture Content 0.080
0.080
wt% water; ASTM E203-96
ASTM Color <= 50
<= 50
APHA; ASTM D4890-93
Thermal Properties Metric English Comments
Flash Point >= 270 °C
>= 518 °F
Pensky Martens closed cup
Chemical Properties Metric English Comments
Total Acid Number 0.20 - 0.50
0.20 - 0.50
[mg KOH/g]; DOWM 100387-TE95A
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 31 - 36
ASTM D4274-94d