Physical Properties Metric English Comments
Specific Gravity 1.091 g/cc
1.091 g/cc
Dow VORANOL™ CP 1421 Polyol
VORANOL™ CP 1421 polyol is a polyether polyol especially designed for the production of soft and hypersoft flexible slabstock foams. It is also used at low level (0.5 to around 5 php) as cell open..