Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil 639 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Mobil 1 20W-50 Motorcycle Oil V-Twin 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Mobil Jet Oil II Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combina.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Mobil Rarus 829 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Mobil Rarus 827 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |
|||
Flash Point | 270 °C | 518 °F | COC |
ConocoPhillips Syncon® 46 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ChevronTexaco 600R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ChevronTexaco Clarity® ISO 460 Synthetic Paper Machine Oil FeaturesChevron Clarity Synthetic Paper Machine Oils combine the unique ashless formulation of Chevron Clarity® Paper Machine Oils with the superior performance properties of polyalphaolefin (PAO) .. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ChevronTexaco HDAX® SAE 40 Medium Ash Gas Engine Oil Chevron HDAX Medium Ash Gas Engine oil is a premium quality, medium ash, dispersant/detergent type gas engine oil formulated especially for Superior and Waukesha four-stroke engines where medium ash.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ChevronTexaco ISO 460 Industrial Oil EP FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long .. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ChevronTexaco MP Drive Train Fluid FeaturesChevron Drive Train Fluid - MP is a multipurpose lubricant designed for use in transmissions, wet brakes, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or TO-4M requiremen.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ChevronTexaco ParaMount™ 6001 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Flash Point | 270 °C | 518 °F | |
ChevronTexaco Pinnacle® 150 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Flash Point | 270 °C | 518 °F | |
ChevronTexaco Pinnacle® 220 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Flash Point | 270 °C | 518 °F | |
ChevronTexaco Pinnacle® 680 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Flash Point | 270 °C | 518 °F | |
ChevronTexaco Taro® 13 ZF SAE 40 Texaco Tar 13 ZF is a high dispersant, zinc free oil designed for turbocharged and naturally aspirated diesel engines. Typical test data are average values only. Minor variations which do not affect.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil 639 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Febis K Series 100 Exxon Febis K Series oils are premium quality lubricants designed to satisfy the strictest requirements of machine tool slideways. Their multi-functional performance makes them suitable for combined.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Mobil 1 20W-50 Motorcycle Oil V-Twin 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Mobil Rarus 827 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Mobil Rarus 829 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |
|||
Flash Point | 270 °C | 518 °F | COC |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 40 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |
|||
Flash Point | >= 270 °C | >= 518 °F | Pensky Martens closed cup |
Dow VORANOL™ CP 1421 Polyol VORANOL™ CP 1421 polyol is a polyether polyol especially designed for the production of soft and hypersoft flexible slabstock foams. It is also used at low level (0.5 to around 5 php) as cell open.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Mobil Jet Oil II Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combina.. |
|||
Flash Point | 270 °C | 518 °F | ASTM D92 |
ExxonMobil Febis K Series 100 Exxon Febis K Series oils are premium quality lubricants designed to satisfy the strictest requirements of machine tool slideways. Their multi-functional performance makes them suitable for combined.. |
|||
Flash Point | 270 °C | 518 °F | |
ChevronTexaco Pinnacle® 320 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Flash Point | 270 °C | 518 °F | |
ChevronTexaco Pinnacle® 460 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Flash Point | 270 °C | 518 °F | COC |
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 40 Conoco® El Mar Ashless Supreme is a premium quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and turbocharged 2-stroke cycle natural gas engines. Engine.. |