Material Notes:
Description: Slightly crystalline, ethylene-propylene-diene (EPDM) terpolymer designed for calendering; offers excellent processing characteristics. Low unsaturation level provides stability during long-term exposures to heat and ultraviolet (UV) light and allows the polymer to be either sulfur or peroxide cured.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.860 g/cc
0.0311 lb/in³
ASTM D297
Volatiles <= 0.40 %
<= 0.40 %
Total Volatiles; DuPont Dow PQ-E-007
Mooney Viscosity 65 - 75

@Temperature 125 °C
65 - 75

@Temperature 257 °F
ML 1 + 4; ASTM D1646
Ash <= 0.10 %
<= 0.10 %
ASTM D5667
Optical Properties Metric English Comments
Yellow Index <= 7.0 %
<= 7.0 %
ASTM E313
Descriptive Properties Value Comments
Contamination Max 20 specks/300 g
DuPont Dow PQ-E-030
ENB 1.4 - 2.2 mass%
ASTM D6047
Ethylene 56.7-59.7 mass%
ASTM D3900
Residual Transition Metal Max 10 ppm
DuPont Dow