Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2280 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance and flexibility, short open time, and high viscosityApplications: Component of hot melt adh.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2330 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance of heat resistance, flexibility and stiffness, medium viscosity, and open timeApplications: Component of.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2715 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, good wetting and tack, and very long open timeApplications: Component of hot melt adhe.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2732 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good tack, and very long open timeApplications: Component of hot mel.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 3180 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Propylene homopolymer and FDA compliantFeatures: Temperature resistance, high melt viscosity, and increased hardnessApplications: Component of modified bi.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 3385 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: High melt viscosity, balanced temperature resistance, and flexibilityApplications: Component of modified bit.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 4304 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Low melt viscosity, moisture barrier, and adhesionApplications: Flooding and filling compounds for wire and cableOther.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 4730 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Excellent low temperature flexibility, lower processing temperature, and superior adhesionApplications: Flooding and f.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 5221 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, ethylene copolymer, and FDA compliantFeatures: High viscosity and low crystallinityApplications: Component of modified bitum.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 1215 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance, short open time, and excellent wetting propertiesApplications: Lamination of reinforced tapes and prot.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2115 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point and short open timeApplications: Component of hot melt adhesives, sealants and specialty.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2180 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point, short open time, good cohesive strength, and high viscosityApplications: Component of h.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 3535 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Excellent low temperature flexibilityApplications: Component of modified bitumen roofing systemsOther Proper.. |
|||
Density | 0.860 - 2.60 g/cc | 0.0311 - 0.0939 lb/in³ | Average value: 1.34 g/cc Grade Count:114 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
Ethylene Propylene Rubber (EPM, EPDM) Satisfactory compatibility with fireproof hydraulic fluids, ketones, hot and cold water, alkalis, and ozone/strong oxidizing chemicals. Unsatisfactory compatibility with most oils, gasoline, kerosen.. |
|||
Density | 0.860 g/cc @Temperature 15.6 °C |
0.0311 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 150 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.860 - 0.900 g/cc | 0.0311 - 0.0325 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ 210 Naphthenic Hydrocarbon Plasticizer Appearance: Clear, free of suspended matterAvailability: North AmericaCAS Number: 64742-53-6Information provided by ExxonMobil |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil 798 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 32 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear® 32 Turbine Oil Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formula.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
BASF 1,2-PDA 1,2-Propylenediamine Formula: C3H10N2CAS: 78-90-0Description: 1,2-Propylenediamine is a colorless liquid, with an amine-like odor. It is also miscible with water in all proportionsSynonyms: 1,2-PDA, 1,2-Propanediamine,.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | Sintered; ASTM D792 |
ALM PS 200 Prototyping Polymer Non-spherical polystyrene powder for production of complex investment casting patterns.PS-200 can be used as a direct drop in replacement for Castform®, and can be successfully blended with Castfor.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil 1 10W-30 Mobil 1 10W-30 is the most advanced performance synthetic engine oil designed to provide the cleaning power, wear protection and performance reserve to keep engines running smooth and clean. Mobil 1.. |
|||
Density | 0.860 g/cc @Temperature 20.0 °C |
0.0311 lb/in³ @Temperature 68.0 °F |
|
Unipetrol PND 33-352-94 Extra Light Fuel Oil Extra light fuel oil si a mix of liquid hydrocarbons obtained from crude oil through distillation and other refining processes, boiling mostly within 150 to 370 °C. It may contain additives to lowe.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil 798 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2780 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good tack, and very long open timeApplications: Component of hot mel.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 5218 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, ethylene copolymer, and FDA compliantFeatures: High viscosity and high ring and ball softening pointApplications: Component .. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
BASF Dibutylethanolamin Formula: C10H23NOCAS:102-81-8Description: Dibutylethanolamine is a colorless to yellow liquid with an amine-like odor.Synonyms: DBEA, 2-Dibutylaminoethanol, Dibutylethanolamine, N,N-Dibutylethanolam.. |