Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy 235 Indium Solder Alloy

Category Metal , Nonferrous Metal , Indium Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 235 Indium Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.59 g/cc
0.310 lb/in³
Thermal Properties Metric English Comments
Melting Point 165 - 195 °C
329 - 383 °F
Solidus 165 °C
329 °F
Liquidus 195 °C
383 °F
Component Elements Properties Metric English Comments
Indium, In 58 %
58 %
Lead, Pb 39 %
39 %
Silver, Ag 3.0 %
3.0 %
Copyright © lookpolymers.com All Rights Reserved