Material Notes:
Dow Polypropylene Homopolymer Resins are semi-crystalline thermoplastic materials that can provide a combination of desirable properties and affordability: low density; excellent chemical resistance and ESCR; excellent moisture barrier; high heat resistance, good gloss; high stiffness and hardness, and low water absorption. Dow Polypropylene Homopolymer resins are suitable for a wide range of applications and may be fabricated by injection molding, blow molding and extrusion.H700-12 Polypropylene Homopolymer resin is suitable for injection molding.Data provided by Dow Chemical.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM Data
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM Data
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
Unannealed; ASTM Data