Dow Corning Z-6040® SILANE

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6040® SILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® Z-6040 Silane is a bifunctional silane containing a glycidoxy reactive organic group and a trimethoxysilyl inorganic group. It is designated ?-glycidoxypropyltrimethoxysilane. This glycidoxy functional silane is reactive with many different types of organic polymers. It is one of a series of organofunctional silanes from Dow Corning Corporation. Other reactive silanes include amines (Dow Corning® Z-6020 and Dow Corning® Z-6026 Silanes), vinyl-benzylamine (Dow Corning® Z-6032 Silane and Dow Corning® Z-6224 Silane), methacrylate (Dow Corning® Z-6030 Silane), vinyl (Dow Corning® Z-6300 Silane, Dow Corning® Z-6518 Silane) and chloropropyl (Dow Corning® Z-6076 Silane).Information provided by Dow Corning
Physical Properties Metric English Comments
Kinematic Viscosity 3.0 cSt
3.0 cSt
Molecular Weight 234 g/mol
234 g/mol
Thermal Properties Metric English Comments
Flash Point 122 °C
252 °F
open cup
Optical Properties Metric English Comments
Refractive Index 1.428
1.428
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Appearance clear