Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 234 g/mol | 234 g/mol | |
Dow Corning Z-6665 SILANE Dow Corning® Z-6665 Silane is high purity, undiluted n-octyltrimethoxy-silane. It can be used undiluted or diluted with an appropriate solvent in the formulation of water repellent products. With p.. |
|||
Molecular Weight | 234 g/mol | 234 g/mol | |
Dow Corning Z-6040® SILANE Dow Corning® Z-6040 Silane is a bifunctional silane containing a glycidoxy reactive organic group and a trimethoxysilyl inorganic group. It is designated ?-glycidoxypropyltrimethoxysilane. This gly.. |