Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 3.0 cSt | 3.0 cSt | |
Lord Adhesives Chemlok® Y-1520A Adhesive LORD Chemlok® Y-1520A adhesive is a clear, one-coat adhesive used to bond specialty elastomers to metal and plastics during vulcanization of the rubber. Chemlok Y-1520A adhesive is useful for bon.. |
|||
Kinematic Viscosity | 3.0 cSt | 3.0 cSt | |
Dow Corning Z-6026 SILANE Dow Corning® Z-6026 Silane is a chemically reactive material composed of an amino-alkyltrimethoxysilane and a polyol diluted to 40% by weight in methanol. Chemically, it is similar to Dow Corning®.. |
|||
Kinematic Viscosity | 3.0 cSt | 3.0 cSt | |
Dow Corning Z-6040® SILANE Dow Corning® Z-6040 Silane is a bifunctional silane containing a glycidoxy reactive organic group and a trimethoxysilyl inorganic group. It is designated ?-glycidoxypropyltrimethoxysilane. This gly.. |