Physical Properties Metric English Comments
Molecular Weight 248.35 g/mol
248.35 g/mol
Dow Corning Z-6030 SILANE
Dow Corning® Z-6030 Silane is a bifunctional silane containing a methacrylate reactive organic group and a trimethoxysilyl inorganic group. The product is designated ?- methacryloxypropyltrimethoxy..