Polymer Property : Kinematic Viscosity = 2.5 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 2.5 cSt

@Temperature 25.0 °C
2.5 cSt

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..
Kinematic Viscosity 2.5 cSt
2.5 cSt
Dow Corning Z-6030 SILANE
Dow Corning® Z-6030 Silane is a bifunctional silane containing a methacrylate reactive organic group and a trimethoxysilyl inorganic group. The product is designated ?- methacryloxypropyltrimethoxy..
Kinematic Viscosity 2.5 cSt
2.5 cSt
3M Fluorinert™ FC-43 Electronic Liquid
3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct..