Dow Corning XIAMETER® PMCPPMX-200 2CS Silicone Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPPMX-200 2CS Silicone Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 200 FLUID 2CS. A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications. INCI Name: DimethiconeInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.870 g/cc

@Temperature 25.0 °C
0.870 g/cc

@Temperature 77.0 °F
Viscosity Measure 2.0 cSt
2.0 cSt
Kinetic/Kinematic
Surface Tension 18.7 dynes/cm
18.7 dynes/cm
Thermal Properties Metric English Comments
Flash Point 87.0 °C
189 °F
Closed Cup
Optical Properties Metric English Comments
Refractive Index 1.39
1.39