Polymer Property : Viscosity Measure = 2.0 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Measure 2.0 - 4.5 cSt
2.0 - 4.5 cSt
Unipetrol Grade B Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..
Viscosity Measure 2.0 - 4.5 cSt
2.0 - 4.5 cSt
Unipetrol Grade D Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..
Viscosity Measure 2.0 cSt
2.0 cSt
Kinetic/Kinematic
Dow Corning XIAMETER® PMCPPMX-200 2CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 2CS. A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications. INCI Name: DimethiconeInf..
Viscosity Measure 2.0 - 4.5 cSt
2.0 - 4.5 cSt
Unipetrol Grade F Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..