Chi Mei Kibipol® PR-040 Butadiene Rubber (HBR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Chi Mei Corporation (ChiMei)
Trade Name Kibipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chi Mei Kibipol® PR-040 Butadiene Rubber (HBR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shoe sole; Tire
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
ASTM D1646
Mooney Viscosity 40 - 50
40 - 50
ASTM D1646
Ash <= 0.50 %
<= 0.50 %
ASTM D1646
Descriptive Properties Value Comments
Apha Color = 10
ASTM D1209
Bale Weight (Kg) 35
Butadiene/Styrene Content (%) 100/0
ASTM D1646
Cis Content (%) = 96
Vinyl Content (%) 1
Wrapping Film (Type) PE