Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® LSR 9390-60 PARTS A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® LSR 9390-60 PARTS A&B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
60 Durometer, 2-part, 1 to 1 mix, oil resistant, tan Liquid Silicone Rubber for injection molding.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc

@Temperature 25.0 °C
1.47 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
Tensile Strength, Ultimate 6.60 MPa
957 psi
Elongation at Break 330 %
330 %
Tear Strength 17.0 kN/m
97.0 pli
Compression Set 15 %
15 %
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Color off-white
Mix Ratio (X:1) 100
Base to Catalyst ETN
Users viewing this material also viewed the following: