Dow Corning SILASTIC® 45563-V SILICONE RUBBER BLACK

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 45563-V SILICONE RUBBER BLACK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
55 Durometer, black, peroxide cured, molding grade Silicone Rubber Compound.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc

@Temperature 25.0 °C
1.15 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
Tensile Strength, Ultimate 8.943 MPa
1297 psi
Elongation at Break 428 %
428 %
Tear Strength 16.8 kN/m
96.0 pli
Descriptive Properties Value Comments
Color black