Dow Corning 734 FLOWABLE SEALANT

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 734 FLOWABLE SEALANT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 1 part solventless silicone elastomer for general sealing and bonding applications. 734 is a flowable liquid that is easy to use and cures on exposure to moisture in the air. Available in clear or in a range of colours.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Volatiles 5.0 %
5.0 %
Mechanical Properties Metric English Comments
Hardness, Shore A 27
27
Tensile Strength, Ultimate 1.500 MPa
217.6 psi
Elongation at Break 315 %
315 %
Thermal Properties Metric English Comments
Brittleness Temperature -65.0 °C
-85.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Strength 17.00 kV/mm
431.8 kV/in
Dissipation Factor 0.00019

@Frequency 100000 Hz
0.00019

@Frequency 100000 Hz
0.00034

@Frequency 100 Hz
0.00034

@Frequency 100 Hz
Descriptive Properties Value Comments
Appearance clear
Color White