Shandong Dongyue Shenzhou New Material Co 3-methoxy-2,2,3,3-tetrafluoropropionatemethylester (MTPME)

Category Other Engineering Material
Manufacturer Shandong Dongyue Shenzhou New Material Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Shenzhou New Material Co 3-methoxy-2,2,3,3-tetrafluoropropionatemethylester (MTPME).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conformable with: Q/DYS 009-2007MTPME is a kind of transparent liquid, aromatic, flammable, stable, nontoxic, easy to decompose at high temperature. It is not only the key intermediate for synthesis of fluorine-containing ether and carboxyl resin, but also a kind of solvent.Main Applications:MTPME is one important intermediate of perfluorocarboxylic resin and raw material of fluoride vinyl ether. It can also be used to prepare adhesion agent, dyestuff, medicine intermediate and polymer. MTPME is also a kind of solvent.Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.
Physical Properties Metric English Comments
Density 1.44 g/cc

@Temperature 25.0 °C
0.0520 lb/in³

@Temperature 77.0 °F
Liquid
Molecular Weight 190 g/mol
190 g/mol
Thermal Properties Metric English Comments
Boiling Point 150 °C

@Pressure 0.1013 MPa
302 °F

@Pressure 14.69 psi
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Chemical Name 3-methoxy-2,2,3,3-tetrafluoropropionatemethylester
Danger Label 3 (flammable)
Molecular Formula CH3OCF2CF2COOCH3
Purity (%) >95