Dow Corning 230 Fluid

Category Polymer , Thermoplastic , Siloxane
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 230 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.012 g/cc

@Temperature 25.0 °C
1.00 - 1.012 g/cc

@Temperature 77.0 °F
Viscosity Measure 1125 - 1645 cSt
1125 - 1645 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point 93.0 °C
199 °F
Closed cup
Optical Properties Metric English Comments
Refractive Index 1.46 - 1.464
1.46 - 1.464
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month