Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.00 - 1.012 g/cc @Temperature 25.0 °C |
1.00 - 1.012 g/cc @Temperature 77.0 °F |
|
Dow Corning 230 Fluid 100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning |