Diamond Polymers NPP 808 C4 TDS Polycarbonate Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP 808 C4 TDS Polycarbonate Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 0.35 %

@Temperature 23.0 °C
0.35 %

@Temperature 73.4 °F
Equilibrium; ASTM D570
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.1 MPa
8140 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 127 %
127 %
ASTM D638
Flexural Modulus 2.163 GPa
313.7 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm,
Temperature 23.0 °C
NB

@Thickness 0.125 in,
Temperature 73.4 °F
reverse notched; ASTM D256
Gardner Impact >= 36.2 J

@Temperature 23.0 °C
>= 26.7 ft-lb

@Temperature 73.4 °F
ASTM D5420
>= 36.2 J

@Temperature -17.8 °C
>= 26.7 ft-lb

@Temperature -0.0400 °F
ASTM D5420
>= 36.2 J

@Temperature -28.9 °C
>= 26.7 ft-lb

@Temperature -20.0 °F
ASTM D5420
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003