Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP 60-763 Clear Amorphous Polyester Copolymer

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP 60-763 Clear Amorphous Polyester Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Water Absorption 0.13 %

@Time 86400 sec
0.13 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 50.0 MPa
7250 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Flexural Strength 70.3 MPa
10200 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm,
Temperature 23.0 °C
NB

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
NB

@Thickness 3.17 mm,
Temperature -30.0 °C
NB

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 33.0 J

@Thickness 3.17 mm,
Temperature 22.8 °C
24.3 ft-lb

@Thickness 0.125 in,
Temperature 73.0 °F
Energy to peak force; ASTM D3763
50.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
37.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
Energy to peak force; ASTM D3763
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 0.80 %
0.80 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Copyright © lookpolymers.com All Rights Reserved