Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2210 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87350 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87850 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid) Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: .. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Oxford Polymers 604-I Polycarbonate/ABS Alloy Polycarbonate/ABS AlloyInformation provided by Oxford Polymers. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ 678UV ASA Available in North America Additive: UV Stabilizer Features: Good Impact Resistance and High Heat ResistanceRoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074.. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | initial |
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th.. |
|||
Flexural Strength | 70.3 MPa @Thickness 3.17 mm |
10200 psi @Thickness 0.125 in |
ASTM D790 |
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 70.3 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
2; ISO 178 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Flexural Strength | 70.3 MPa @Thickness 3.17 mm |
10200 psi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 70.3 MPa @Thickness 3.17 mm |
10200 psi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 70.3 MPa @Thickness 3.17 mm |
10200 psi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 70.3 MPa @Thickness 3.17 mm |
10200 psi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Chase Plastics CP Pryme® AH120 Acetal Copolymer, 20% Glass Fiber Reinforced Form: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers Centrex® 810 Injection Molding Grade Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and .. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers NPP 60-763 Clear Amorphous Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Aremco Aremco-Bond™ 631 High Performance Epoxide Clear-Amber, 1:1, Good Bond Strength and Corrosion Resistance.Also available filled with aluminum oxide (Alumina) or pigments. |
|||
Flexural Strength | 70.3 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |