Denka VINYKON M7300 PVC, M grade for soft injection molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON M7300 PVC, M grade for soft injection molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.368 g/cc
0.04942 lb/in³
JIS-Z-8807
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
JIS-K-6301
Tensile Strength at Break 14.715 MPa
2134.2 psi
JIS-K-6723
Elongation at Break 310 %
310 %
JIS-K-6723
100% Modulus 0.00981 GPa
1.42 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -21.0 °C
-5.80 °F
JIS-K-6723
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 100
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 95
JIS-A-5756