Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.715 MPa | 2134.2 psi | JIS-K-6723 |
Denka REOMER G G5082 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Tensile Strength at Break | 14.715 MPa | 2134.2 psi | JIS-K-6723 |
Denka VINYKON M7100 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Tensile Strength at Break | 14.715 MPa | 2134.2 psi | JIS-K-6723 |
Denka VINYKON M7300 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Tensile Strength at Break | 14.715 MPa | 2134.2 psi | JIS-K-6723 |
Denka VINYKON W7100i PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |