20% Whisker Reinforced, Wear and Friction Modified
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
dry; ISO 1183
Moisture Absorption 2.90 %
2.90 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
0.0090 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 110 MPa
16000 psi
dry; ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
dry; ISO 527-1/-2
Tensile Modulus 7.00 GPa
1020 ksi
dry; ISO 527-1/-2
Flexural Modulus 6.00 GPa
870 ksi
dry; ISO 178
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
dry; ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.790 mm
HB

@Thickness 0.0311 in
dry; IEC 60695-11-10
Users viewing this material also viewed the following: