Material Notes:
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.Information provided by the manufacturer, Brueggemann Chemical.
Physical Properties Metric English Comments
Density 1.322 g/cc
0.04776 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ISO 868
Tensile Strength, Ultimate 28.0 MPa
4060 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Modulus of Elasticity 1.82 GPa
264 ksi
ISO 527
Flexural Modulus 1.98 GPa
287 ksi
ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
DIN 53453
0.500 J/cm²

@Temperature -40.0 °C
2.38 ft-lb/in²

@Temperature -40.0 °F
DIN 53453