Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Arnite® TV4 640 (PBT+PC) - GF20

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® TV4 640 (PBT+PC) - GF20.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Glass Reinforced
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 110 MPa
16000 psi
ISO 527-1/-2
Elongation at Break 2.8 %
2.8 %
ISO 527-1/-2
Tensile Modulus 6.50 GPa
943 ksi
ISO 527-1/-2
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 183 °C
361 °F
ISO 75-1/-2
Users viewing this material also viewed the following: