Material Notes:
30% Glass Reinforced, Halogen free and free of red phosphorous
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
dry; ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 150 MPa
21800 psi
dry; ISO 527-1/-2
Elongation at Break 2.8 %
2.8 %
dry; ISO 527-1/-2
Tensile Modulus 11.0 GPa
1600 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 6.30 J/cm²

@Temperature 23.0 °C
30.0 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
dry; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
dry; IEC 60695-11-10
V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
dry; IEC 60695-11-10