Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cytec Thornel® VCB-20 Carbon Cloth/Epoxy Composite

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite , Filled/Reinforced Thermoset
Manufacturer Cytec
Trade Name Thornel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Thornel® VCB-20 Carbon Cloth/Epoxy Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc. Cured ply 0.47 mm thick, 55% fiber vol.Thornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 275 MPa
39900 psi
Tensile Modulus 41.0 GPa
5950 ksi
Flexural Yield Strength 380 MPa
55100 psi
Flexural Modulus 38.0 GPa
5510 ksi
Compressive Yield Strength 345 MPa
50000 psi
Shear Strength 35.0 MPa
5080 psi
Short Beam
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C

@Temperature 20.0 °C
5.00 µin/in-°F

@Temperature 68.0 °F