Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 275 MPa
>= 39900 psi
MetalTek MTEK 20% Ni 412 Cast UNS C97600 Nickel-Silver
Information provided by MetalTekCast UNS C97600; Cast Grade C97600; Cast ASTM B271, B584; Military MIL-C-17112
Tensile Strength, Ultimate >= 275 MPa
>= 39900 psi
MetalTek NAVY G Cast UNS C90300 Bearing Bronze
Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C90300; Cast Grade C90..
Tensile Strength, Ultimate >= 275 MPa
>= 39900 psi
MetalTek MTEK 87-11-1-0-1 Cast UNS C92500 Gear Bronze
Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C92500; Cast Grade C92..
Tensile Strength, Ultimate 275 MPa

@Temperature 980 °C
39900 psi

@Temperature 1800 °F
Haynes 25 alloy, cold worked sheet, 15 % cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 275 MPa
39900 psi
Wieland 1651 Wilaform Gold
High-quality alloy for all kinds of decoration production.Applications: casting, coin/shape, laminar decoration, pipes, tubingDental
Tensile Strength, Ultimate 275 MPa
39900 psi
ACMA Test #4
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Tensile Strength, Ultimate 275 MPa
39900 psi
Cytec Thornel® VCB-20 Carbon Cloth/Epoxy Composite
Data provided by the manufacturer, Amoco Performance Products, Inc. Cured ply 0.47 mm thick, 55% fiber vol.Thornel® products were sold by Amoco and are now owned by Cytec.
Tensile Strength, Ultimate 275 - 440 MPa
39900 - 63800 psi
ArcelorMittal 11 High formability steel for drawing, Hot rolled
Available in the following: uncoated (DD11) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au..
Tensile Strength, Ultimate >= 275 MPa
>= 39900 psi
Rm
ALIMEX 6082 T651 Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then artificially aged.
Tensile Strength, Ultimate 275 MPa
39900 psi
ASTM D638
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC  (discontinued **)
QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and ..
Tensile Strength, Ultimate 275 MPa
39900 psi
ASTM D638
Quantum Composites QC-8704FR 63% Glass Fiber Flame Retardant Vinyl Ester SMC  (discontinued **)