| Category | Polymer , Renewable/Recycled Polymer , Thermoplastic |
| Manufacturer | Cyclewood Solutions |
| Trade Name | Xylomer™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Cyclewood Solutions Xylomer™ XM2-FPC Sustainable Injection Molding Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.068 g/cc | 0.03858 lb/in³ | |
| Melt Flow | 15.6 g/10 min @Temperature 230 °C |
15.6 g/10 min @Temperature 446 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 28.17 MPa | 4085 psi | |
| Elongation at Break | 3.0 % | 3.0 % | |
| Flexural Modulus | 1.72 GPa | 250 ksi | |
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in |