Covestro Bayflex® 110-50 CM Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Covestro
Trade Name Bayflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayflex® 110-50 CM Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
Bayer Test
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength, Ultimate 23.0 MPa
3340 psi
ASTM D638/D412
Elongation at Break 360 %
360 %
ASTM D638/D412
Flexural Modulus 0.320 GPa
46.4 ksi
ASTM D790
Izod Impact, Notched 4.80 J/cm
8.99 ft-lb/in
ASTM D256
Tear Strength 87.0 kN/m
496 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
CTE, linear 153 µm/m-°C

@Temperature 20.0 °C
85.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Flammability, UL94 V-2

@Thickness 3.18 mm
V-2

@Thickness 0.125 in
V-2

@Thickness 3.18 mm
V-2

@Thickness 0.125 in