Material Notes:
GRAFOIL® TG-411 is a high temperature purified flexible graphite sheet for applications that require extremely low impurity levels. Material greater than 0.040" (1 mm) thick is adhesively bonded to final thickness, followed by the purification process.
Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Available
Thickness 250 - 760 microns
9.84 - 29.9 mil
Available Range
Component Elements Properties Metric English Comments
Aluminum, Al 0.00010 %
0.00010 %
Arsenic, As <= 1.0e-6 %
<= 1.0e-6 %
Boron, B 0.0000070 %
0.0000070 %
Calcium, Ca <= 0.00010 %
<= 0.00010 %
Chlorine, Cl <= 0.000050 %
<= 0.000050 %
Chromium, Cr <= 0.000010 %
<= 0.000010 %
Cobalt, Co <= 0.0000050 %
<= 0.0000050 %
Copper, Cu <= 0.0000050 %
<= 0.0000050 %
Germanium, Ge <= 0.000010 %
<= 0.000010 %
Iron, Fe 0.00030 %
0.00030 %
Lithium, Li 0.000010 %
0.000010 %
Magnesium, Mg 0.00010 %
0.00010 %
Manganese, Mn 0.000010 %
0.000010 %
Mercury, Hg <= 0.000050 %
<= 0.000050 %
Nickel, Ni 0.000030 %
0.000030 %
Phosphorous, P 0.00015 %
0.00015 %
Potassium, K 0.00010 %
0.00010 %
Selenium, Se <= 0.000010 %
<= 0.000010 %
Silicon, Si 0.00050 %
0.00050 %
Sodium, Na 0.00020 %
0.00020 %
Sulfur, S 0.00020 %
0.00020 %
Tantalum, Ta <= 0.00050 %
<= 0.00050 %
Titanium, Ti 0.000010 %
0.000010 %
Zinc, Zn <= 0.0000050 %
<= 0.0000050 %
Descriptive Properties Value Comments
Bromine, Br (%) <0.00001
Total Impurities (%) <0.0020