Material Notes:
Mechanical Properties Metric English Comments
Flexural Strength 3.10 MPa
450 psi
Compressive Strength 31.0 MPa
4500 psi
Thermal Properties Metric English Comments
CTE, linear 4.68 µm/m-°C

@Temperature 20.0 °C
2.60 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.576 W/m-K
4.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1540 °C
2800 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Dielectric Strength 10.6 kV/mm
270 kV/in