Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 140 MPa | 20300 psi | |
Poco Graphite DFP Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Compressive Strength | 140 MPa | 20300 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Compressive Strength | 140 MPa | 20300 psi | 5% Def.; ISO 604 |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
Compressive Strength | 140 MPa | 20300 psi | Edgewise; ASTM D695 |
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3) Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product. |
|||
Compressive Strength | 140 MPa | 20300 psi | Cold Crushing Strength |
Gouda Vuurvast ACZ 85-5 D Dense Refractory Brick Description: Special low porosity quality with excellent resistance against alkali- and metal slags, a good volume stability and a high strength and elasticity at very high temperatures. Application.. |
|||
Compressive Strength | 140 MPa | 20300 psi | ISO 604 |
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 140 MPa | 20300 psi | ISO 604 |
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 140 MPa | 20300 psi | ASTM D695 |
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate Long glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type GDI-30F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | 140 MPa | 20300 psi | ASTM D695 |
Plenco 08122 Polyester BMC, Compression Molded PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Compressive Strength | 140 MPa | 20300 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | 140 MPa | 20300 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | 140 MPa | 20300 psi | ASTM C773 |
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Compressive Strength | 140 MPa @Temperature 23.0 °C, Time 86400 sec |
20300 psi @Temperature 73.4 °F, Time 24.0 hour |
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2 |
Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: A strong and tough material. Very low water absorption and the lowest swelling in water. Very good low-friction material. High wear resistance in aggressive and dust-filled environments.. |
|||
Compressive Strength | 140 MPa @Temperature 23.0 °C, Time 86400 sec |
20300 psi @Temperature 73.4 °F, Time 24.0 hour |
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2 |
Elektro-Isola Etronit B 65 Phenolic, Paper Reinforcement, Dark Brown, Tubes Description: For mechanical and electrical low-voltage applications. Good electrical properties at normal air humidity.Applications: Winding tubes in the foil and metal foil industries and carrier t.. |
|||
Compressive Strength | 140 MPa @Temperature 23.0 °C, Time 86400 sec |
20300 psi @Temperature 73.4 °F, Time 24.0 hour |
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2 |
Elektro-Isola Etronit B67 Phenolic, Paper Reinforcement, Dark Brown, Tubes Description: For mechanical and electrical low-voltage applications. Very good electrical properties at high air humidity. Applications: Winding tubes in the foil and metal foil industries and carri.. |
|||
Compressive Strength | 140 - 160 MPa | 20300 - 23200 psi | ISO 604 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Compressive Strength | 140 - 180 MPa | 20300 - 26100 psi | ISO 604 |
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot.. |
|||
Compressive Strength | 140 - 200 MPa | 20300 - 29000 psi | ISO 604 |
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote.. |
|||
Compressive Strength | 140 MPa | 20300 psi | ASTM D695 |
Plenco 7321 Phenolic, Nodular, Compression Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Compressive Strength | 140 MPa | 20300 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owen.. |
|||
Compressive Strength | 140 MPa @Temperature 23.0 °C |
20300 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® MD 100 Pattern material Densified laminated woodInformation provided by elisto |