Material Notes:
The Polycom VY series are compounds for the extrusion of both stripes for chaise lounge and flexible window sidings with outstanding weather and outdoes resistance. Also, in the VY series the are products for the extrusion of profiles for refrigerators.Applications: Flexible profile extrusion Appearance: Natural pelletsInformation provided by Compuestos Dominicanos
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.48 g/cc
1.44 - 1.48 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 71 - 75

@Time 15.0 sec
71 - 75

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 17.9 MPa
2600 psi
ASTM D412
Elongation at Break 720 %
720 %
ASTM D412