Compuestos Dominicanos Polycom VN-050485 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Compuestos Dominicanos, S.A. (polycom)
Trade Name Polycom
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Compuestos Dominicanos Polycom VN-050485 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Compuestos Dominicanos manufactures the polycom VN products for the extrusion printable sheets and banners having good printing quality.Application: Sheet and bannersAppearance: Natural PelletsInformation provided by Compuestos Dominicanos, S.A.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 86
82 - 86
15 seconds; ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D412
Elongation at Break 596 %
596 %
ASTM D412