Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.30 g/cc
0.119 lb/in³
Porosity 15 %
15 %
Mechanical Properties Metric English Comments
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 7.80 µm/m-°C

@Temperature 1000 °C
4.33 µin/in-°F

@Temperature 1830 °F
Shrinkage 0.00 %

@Temperature 1500 °C,
Time 7200 sec
0.00 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 99 %
99 %
Fe2O3 0.10 %
0.10 %
Descriptive Properties Value Comments
Main Application Ammonia plant, Carbon Productor, Rotary kiln, Shaft kiln, Various high-temp. furnace
Refractories Under Load(2kg/?,T2?) 1,700 T1
Refractoriness (SK) 42