Polymer Property : Compressive Strength = 12800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 88.0 MPa
12800 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 510 Polyethylene Terephthalate
Application: friction bearings, wear linersInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing
Sharadaa Ceramics PCF (SIC) Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing
Sharadaa Ceramics PCF60-2 Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing
Sharadaa Ceramics PCF70 Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing
Sharadaa Ceramics PCF80 Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing
Sharadaa Ceramics PCF90 Precast Prefired Brick
Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin..
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing
Sharadaa Ceramics HA 88X High Alumina Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 88.0 MPa
12800 psi
ASTM D695
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound
Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information ..
Compressive Strength 88.0 MPa
12800 psi
ASTM D695
Sumitomo Bakelite North America SI 9550 Silicone Compound
SI 9550 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated tempera..
Compressive Strength 88.3 MPa
12800 psi
ASTM D695
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound
Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It ..
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories COD-2 Special brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 88.3 MPa
<= 12800 psi
Cold Crushing Strength
Chosun Refractories CUN-B937 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories SAL85N Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories SAL90 Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories SAL90CR Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories SAL95S Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories SAL99 Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories SAL99C Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories SB65S Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories SC80 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Chosun Refractories AH-1 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.0 MPa
12800 psi
ASTM D695
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound
SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp..