Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.00 g/cc
0.108 lb/in³
Porosity 17 %
17 %
Mechanical Properties Metric English Comments
Compressive Strength 83.4 MPa
12100 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 7.20 µm/m-°C

@Temperature 1000 °C
4.00 µin/in-°F

@Temperature 1830 °F
Shrinkage 0.00 %

@Temperature 1600 °C,
Time 7200 sec
0.00 %

@Temperature 2910 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 86 %
86 %
Cr2O3 5.0 %
5.0 %
Descriptive Properties Value Comments
Main Application Hot blast Stove, Chemical Reactor, Incinerator, Glass melting Tank
Refractories Under Load(2kg/?,T2?) 1,700
Refractoriness (SK) 40