Chosun Refractories HSM-38 Heat-Setting Mortar

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories HSM-38 Heat-Setting Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Grain Size 75 µm
75 µm
50% <= 0.075 mm
300 µm
300 µm
5% >= 0.30 mm
Component Elements Properties Metric English Comments
Al2O3 70 - 75 %
70 - 75 %
Fe2O3 >= 3.0 %
>= 3.0 %
SiO2 20 - 25 %
20 - 25 %
Processing Properties Metric English Comments
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Descriptive Properties Value Comments
Main Applications SK38 Bricks
Refractoriness (SK) 38=