ChevronTexaco FM ISO 460 Lubricating Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name FM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco FM ISO 460 Lubricating Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubricating Oils FM provide performance well above that found in typical white mineral oils often used in the food industry. They contain a special biocide to prevent growth of molds when the product comes in contact with food or water.ApplicationsGear setsrotary steamersvalves up to 175°C (350°F)
Physical Properties Metric English Comments
API Gravity 29.2 °
29.2 °
Viscosity Measurement 118
118
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 2308 SUS
2308 SUS
Saybolt Viscosity at 210°F 169 SUS
169 SUS
Kinematic Viscosity at 40°C (104°F) 437 cSt
437 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 34.7 cSt
34.7 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Wear 0.430 mm
0.0169 in
Thermal Properties Metric English Comments
Pour Point -9.00 °C
15.8 °F
ASTM D97
Flash Point 243 °C
469 °F
ASTM D92
Descriptive Properties Value Comments
Rust preventative Test Procedure B Pass
Synthetic Sea Water