Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 169 SUS
169 SUS
ChevronTexaco FM ISO 460 Lubricating Oil
Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr..
Saybolt Viscosity at 210°F 169 SUS
169 SUS
ChevronTexaco Syn-Star® 320 Chain Oil
Texaco Syn-Star Chain Oil 320 is a chain oil designed for use in extreme high and low temperature operations. It is formulated with synthetic base oils and an additive package which provides rust an..