Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low density linear polyethylene. This low density, linear resin is tailored for blow molded containers that require: Excellent processabilityExcellent ESCRApplications: Typical blow molded applications for HHM TR-232 include: Squeezable bottlesLarge flexible partsTraffic barrelsInformation provided by PhillipsThis resin meets these specifications: ASTM D4976 - PE 215FDA 21 CFR 177.1520(c) 3.1a, use conditions C through G per 21 CFR 176.170(c)
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D-1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Condition A, F50; ASTM D-1693
>= 1000 hour
>= 1000 hour
Condition B, F50; ASTM D-1693
Melt Flow 18 g/10 min
18 g/10 min
HLMI, 190/21.6; ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.0 MPa
1890 psi
2 in/min, Type IV bar; ASTM D-638
Elongation at Break 800 %
800 %
2 in/min, Type IV bar; ASTM D-638
Flexural Modulus 0.480 GPa
69.6 ksi
Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A, Type I specimen; ASTM D-746